Cyryl Plotnicki-Chudyk
|
113100ae63
|
legacy reprap slic3r settings removed, only one known good retained
|
2014-10-25 09:58:33 +02:00 |
|
Cyryl Plotnicki-Chudyk
|
038d192a32
|
use multiplier of 1 for extrusion, as E-steps tuned
|
2014-10-25 09:55:34 +02:00 |
|
Cyryl Plotnicki-Chudyk
|
ca03571492
|
flow rate adjusted for pink abs
|
2014-10-23 21:55:38 +02:00 |
|
Cyryl Plotnicki-Chudyk
|
824a5cf5de
|
less plastic flowing, slightly slower prints, always cool prints
|
2014-10-23 20:21:31 +02:00 |
|
Cyryl Plotnicki-Chudyk
|
3e51f78cf0
|
slightly higher bed temperature for abs prints to avoid warping on the larger ones
|
2014-10-16 18:13:21 +02:00 |
|
Cyryl Plotnicki-Chudyk
|
99053adbf7
|
rise bed temperature during print, as small ones tend to have the devil's horns visible
|
2014-10-11 22:04:20 +02:00 |
|
Cyryl Plotnicki-Chudyk
|
b181262fdf
|
new pink abs settings
|
2014-10-11 13:22:54 +02:00 |
|
Cyryl Plotnicki-Chudyk
|
3f94977f91
|
colder bed for abs as buildtakk in use
|
2014-09-23 18:55:45 +02:00 |
|
Cyryl Plotnicki-Chudyk
|
9b48f88888
|
slightly less warm nozzle for black pla
|
2014-08-17 12:08:29 +02:00 |
|
Cyryl Plotnicki-Chudyk
|
8c603ed0af
|
cleaned up unused slic3r files
|
2014-08-17 10:22:58 +02:00 |
|
Cyryl Plotnicki-Chudyk
|
c09c1c917e
|
another tries at printing pink abs
|
2014-08-16 14:21:33 +02:00 |
|
Cyryl Plotnicki-Chudyk
|
f2a06e4712
|
trying to find best settings for pink abs printing
|
2014-08-09 10:03:57 +02:00 |
|
Cyryl Plotnicki-Chudyk
|
408c6cef1a
|
slic3r dotfiles added
|
2014-08-09 07:33:56 +02:00 |
|